mercurymang
Master Chief Petty Officer
- Joined
- Jul 14, 2012
- Messages
- 853
Re: 1974 Ebbtide Restoration
Re: 1974 Ebbtide Restoration
Cool
This is the exact measuring cup that came with my hardener from USC. I went to a pharmacy the other day and asked for some of these and they said they did not have any. I guess I'll try somewhere else.
BTW, I thought that if you don't use any wax, the outer portion of your resin will remain tacky for a while. The sample I created last night is now hard as a rock and tackfree as glass.
Re: 1974 Ebbtide Restoration
Next time you place an order for glassing materials, get a catalyst dispenser like this one.
![]()
The top cup is graduated in mL (CC's), you just squeeze the bottle until you have the desired amount in the top cup, then pour into your mix. It's a real time saver, in my opinion, and helps keeping you from making mistakes with the ratio. I think it costs around $6, so why the heck not. I can't imagine how much time it's saved me along the way.
Cool
Or go to the drug store and get some of these. They're real cheap too... $5 bucks for 100 of em.![]()
This is the exact measuring cup that came with my hardener from USC. I went to a pharmacy the other day and asked for some of these and they said they did not have any. I guess I'll try somewhere else.
BTW, I thought that if you don't use any wax, the outer portion of your resin will remain tacky for a while. The sample I created last night is now hard as a rock and tackfree as glass.