got a 22' cruiser that sat for years outside being abused, it had alot of growth all over the topside "moss". I used a pressure washer to remove all the moss and cleaned it real well I used Muriatic acid "with scrubbing" and also some commercial cleaner, butu i still have dark Yellow staining on the topside from where the moss was growing/ decaying. Does anyone have any idea how to remove this yellow staining. "cannot sand it out cuz it is on Non skid areas" also while pressure washing i removed some of the old gel coat and glass after fixing can i re gel just these areas or do i need to re gel entire boat? and lastly can i regel a boat over existing Good gel as long as it is sanded first?