Something very odd is going on with my boat and its 7.4L/Bravo III setup that I do not understand at all. It has only started happening upon boating in the Great Lakes and plugging in at Michigan municipal (hot?!) marinas.
Here is some backstory: Soul Rebel became a freshwater boat in 2023. Before so doing, i changed all of her anodes to magnesium, including for her trim tabs. I replaced her Mercathode in 2020/21 (I forget which). I installed a basic "shorepower system" in 2022 which is basically just a plug that goes to a battery charger that I use with a 25' cord with a built-in 15 AMP GFCI breaker that I plug into the dock with a 30 amp to 15 amp adapter--I only use this to keep the battery charged and all lights, fridge, etc. are 12 volt and run off the battery.
Since 2023, she has spent about 15 overnights in various marinas plugging into dock pedestals. After getting back from our last jaunt, I noticed some serious corrosion on the gimbal ring near the steering pin that I had never noticed before (see pics). I will sand, prime, and paint it and the outdrive (as I have done before) next season, but I want to solve the issue.
Digging around the boat and bit more, I have noticed some corrosion on the engine block and steering arm (since it is bonded to the gimbal ring I imagine). The underwater stainless surfaces are also a bit pitted and some have some rust (see pictures); all underwater stainless has this white film on it. It is like the entire anode/bonding system is not working despite all of the wires being connected and intact (see pictures). The anodes are also not corroding one iota which I do not get despite them being magnesium from martyr and/or boatzincs.
I am at a loss and hope the galvanic activity has not damaged my water jackets or other internal engine water passages! Any input would be appreciated. @tpenfield @Lou C










Here is some backstory: Soul Rebel became a freshwater boat in 2023. Before so doing, i changed all of her anodes to magnesium, including for her trim tabs. I replaced her Mercathode in 2020/21 (I forget which). I installed a basic "shorepower system" in 2022 which is basically just a plug that goes to a battery charger that I use with a 25' cord with a built-in 15 AMP GFCI breaker that I plug into the dock with a 30 amp to 15 amp adapter--I only use this to keep the battery charged and all lights, fridge, etc. are 12 volt and run off the battery.
Since 2023, she has spent about 15 overnights in various marinas plugging into dock pedestals. After getting back from our last jaunt, I noticed some serious corrosion on the gimbal ring near the steering pin that I had never noticed before (see pics). I will sand, prime, and paint it and the outdrive (as I have done before) next season, but I want to solve the issue.
Digging around the boat and bit more, I have noticed some corrosion on the engine block and steering arm (since it is bonded to the gimbal ring I imagine). The underwater stainless surfaces are also a bit pitted and some have some rust (see pictures); all underwater stainless has this white film on it. It is like the entire anode/bonding system is not working despite all of the wires being connected and intact (see pictures). The anodes are also not corroding one iota which I do not get despite them being magnesium from martyr and/or boatzincs.
I am at a loss and hope the galvanic activity has not damaged my water jackets or other internal engine water passages! Any input would be appreciated. @tpenfield @Lou C