Re: New owner of a 91 Maxum 1800 have a few questions
a few questions,
The spot repairs, there was no damage to the glass, just the gelcoat. I sanded down all the way through the white gelcoat when cleaning the old repair material off. Are you saying i need to lay glass down there too, or just on the keel?
Do i need to grind down more where the glass is already showing on the keel, or are you just saying i need to go out to the sides more to remove more gelcoat?
Do i wait for the filler to cure before putting the first csm mat on?
I would say the big areas on the keel total 36 inches long by 2 inches wide. How much csm, 1708 and resin and gelcoat do i need? The gelcoat area is probably about 7-8 inches wide down pretty much the entire length. I would say 4-5 feet long
Also,
how long after i do all of this before i can put it in the water?
a few questions,
The spot repairs, there was no damage to the glass, just the gelcoat. I sanded down all the way through the white gelcoat when cleaning the old repair material off. Are you saying i need to lay glass down there too, or just on the keel?
Do i need to grind down more where the glass is already showing on the keel, or are you just saying i need to go out to the sides more to remove more gelcoat?
Do i wait for the filler to cure before putting the first csm mat on?
I would say the big areas on the keel total 36 inches long by 2 inches wide. How much csm, 1708 and resin and gelcoat do i need? The gelcoat area is probably about 7-8 inches wide down pretty much the entire length. I would say 4-5 feet long
Also,
how long after i do all of this before i can put it in the water?