My procedure is a bit less labor intensive and more geared towards a boat you use rather than a perfect trailer queen for parades. I use the wet on wet method of painting. After I sand the hull with 220g using palm sander to break the surface tension and create more area for the SE primer to grab I wash the hull down with cleaning vinegar then rinse well with clean water and wipe with lint free towels.
Once the hull is dried I start the process.
SE primer one coat to cover well. Clean HVLP gun and then shoot a nice coat of regular primer. Clean HVLP gun and have some refreshments. Mix paint with reducer and catalyst hardener, let cook 20 min and then shoot the first paint coat. Clean HVLP gun, relax for an hour or so and mix the second coat of paint up. When cook time is up I shoot the second and final coat of paint. Done in one long sticky day and NO sanding. If doing an accent stripe then the next day if the paint is set up good I tape off the area and shoot the stripe wait an hour, shoot the second coat and after 2 hours pull the tape.
I hate sanding and have never claimed my paint jobs are perfect but the results are tough as nails after total curing for a month or so and then the 303 quick wax goes on. You can check out my threads and see the results and make up your mind on how too proceed.