NatedoggAZ
Petty Officer 2nd Class
- Joined
- Mar 7, 2018
- Messages
- 182
After I make the PB fillet (or whatever it is called) how long should I wait before applying the first layer of 1708 glass?
Should I apply the 1708 while the PB has just been put in and is still in its original PB consistency?
Should I wait until it hardens a little and is still tacky?
or Should I wait until it is completely dry?
...this is the PB that is from hull to stringer...if that matters...
Thanks!
ND
Should I apply the 1708 while the PB has just been put in and is still in its original PB consistency?
Should I wait until it hardens a little and is still tacky?
or Should I wait until it is completely dry?
...this is the PB that is from hull to stringer...if that matters...
Thanks!
ND