I have just purchased all of my fiberglass supplies and need a refresher on the exact process:
Questions I have:
1.) For the bottom of the deck: Does the resin go on first or the glass? Also, which resin (the waxed or unwaxed)?
2.) Can someone explain the process for both sides: Like, what resin goes on when and the order of things. Looking for 1 layer 1.5 oz csm on bottom and 2 layers on top with waxed final resin.
I bought 1 gallon of waxed and 2 gallons of unwaxed. I was thinking it would just be 1 coat of waxed for the last layer on the top of the deck. Not sure.
3.) Can I just put 1 layer of waxed on the bottom and not glass it?
Basically I need to do a deck with seat bases. Total area is approx 30sq ft per side. I only assumed it would be a total of 3 coats of wax (1 unwaxed on bottom, 1 unwaxed on top and 1 waxed top). I may have messed up on this though. Bought 95sq ft of csm.
If I can avoid glassing the bottom I should have plenty. Any help would be great. Thanks!
Questions I have:
1.) For the bottom of the deck: Does the resin go on first or the glass? Also, which resin (the waxed or unwaxed)?
2.) Can someone explain the process for both sides: Like, what resin goes on when and the order of things. Looking for 1 layer 1.5 oz csm on bottom and 2 layers on top with waxed final resin.
I bought 1 gallon of waxed and 2 gallons of unwaxed. I was thinking it would just be 1 coat of waxed for the last layer on the top of the deck. Not sure.
3.) Can I just put 1 layer of waxed on the bottom and not glass it?
Basically I need to do a deck with seat bases. Total area is approx 30sq ft per side. I only assumed it would be a total of 3 coats of wax (1 unwaxed on bottom, 1 unwaxed on top and 1 waxed top). I may have messed up on this though. Bought 95sq ft of csm.
If I can avoid glassing the bottom I should have plenty. Any help would be great. Thanks!
Last edited: